What is grade 316L stainless steel?

Jan 28, 2026

Lasciate un messaggio

What is 1.4546 Stainless Steel?What is 1.4568 Stainless Steel?What Is 321 (UNS S32100) Stainless Steel

 

 

  C P S N
316 (S31600) 0.08 max 2.0 max 0.75 max 0.045 max 0.03 max

min: 16.0

max: 18.0

min: 2.0

max: 3.0

min: 10.0

max: 14.0

0.10 max
316L (S31603) 0.03 max 2.0 max 0.75 max 0.045 max 0.03 max

min: 16.0

max: 18.0

min: 2.0

max: 3.0

min: 10.0

max: 14.0

0.10 max

 

 

 

Yield Strength 0.2% ksi (min)

316

(S31600)

75 30 40 217 95

316L

(S31603)

70 25 40 217 95

 

 

 

Density lbm/in3 Thermal Conductivity (BTU/h ft. ℃F) Electrical Resistivity (in x 10-6) Modulus of Elasticity (psi x 10-6) Coefficient of Thermal Expansion (in/in)/℃F x 10-6)
0.29 at 68℃F 100.8 at 68 212℃F 29.1 at 68℃F 29 8.9 at 32 – 212℃ 0.108 at 68℃F 2500 to 2550
        9.7 at 32 – 1000℃ 0.116 at 200℃F  
        11.1 at 32 – 1500℃    